• HW series (Water-based modified acrylic carrier)

    HW series (Water-based modified acrylic carrier)

    Usage of HW Series Pigment chip :  25-33% Water or Ethanol: 67-75% Mixing time: 25±2 min. Stirring Speed: 1200±50 r/min Usage: First add water or ethanol into the container,  and slowly stir, slowly add all the pigment chips, then increase the speed to high.

  • HSC series (Modified acrylic carrier)

    HSC series (Modified acrylic carrier)

    Usage of HSC Series Pigment chip :  25-33% Water: 67-75% DEA: 3-5% Mixing time: 20-25min. Stirring Speed: 1000-1500r/min Usage: First add water and DEA into the container,  and slowly stir, slowly add all the pigment chips, then increase the speed to high.

  • HST series (Modified acrylic carrier)

    HST series (Modified acrylic carrier)

    Usage of HST Series Pigment chip :  25-33% Water: 67-75% DEA: 3-5% Mixing time: 20-25min. Stirring Speed: 1000-1500r/min Usage: First add water and DEA into the container,  and slowly stir, slowly add all the pigment chips, then increase the speed to high.

  • HCC series (Alcohol solvent high polymer resin carrier)

    HCC series (Alcohol solvent high polymer resin carrier)

    Usage of HCC Series Pigment chip :  10% Ink resin: 90% Mixing time: 20-25min. Stirring Speed: 1000-1500r/min Recommended Solvent: ethanol or 2-Butoxyethanol. Usage:First pour solvent into the container and slowly stir, slowly add all the pigment chips, then increase the speed to high.

  • HPU series (High polymer resin carrier)

    HPU series (High polymer resin carrier)

    Usage of HPU Series Pigment chip :  10-15% Ink resin: 85-90% Mixing time: 20-25min. Stirring Speed: 1000-1500r/min Usage: Dissolve the Pigment chip directly in PU resin, stir and dissolve completely.